000000055 001__ 55 000000055 005__ 20231130114534.0 000000055 0247_ $$2DOI$$a10.6083/M4W37T83 000000055 037__ $$aETD 000000055 245__ $$aEffects of microstructure on the internal hydrogen embrittlement of a 4340 steel 000000055 260__ $$bOregon Graduate Center 000000055 269__ $$a1980 000000055 336__ $$aDissertation 000000055 502__ $$bPh.D. 000000055 540__ $$fCC BY 000000055 542__ $$fIn copyright - single owner 000000055 650__ $$aSteel$$026389 000000055 6531_ $$amicrostructure 000000055 6531_ $$ahydrogen embrittlement 000000055 692__ $$aDepartment of Materials Science and Engineering$$041420 000000055 7001_ $$aBauer, Charles E. 000000055 7001_ $$uOregon Graduate Center$$041351 000000055 8564_ $$9187c1213-d56e-4149-a9a2-2629ae59c452$$s2446022$$uhttps://digitalcollections.ohsu.edu/record/55/files/55_etd.pdf 000000055 905__ $$a/rest/prod/r4/94/vk/16/r494vk167 000000055 909CO $$ooai:digitalcollections.ohsu.edu:55$$pstudent-work 000000055 980__ $$aTheses and Dissertations